| CLASSIFICATION |
|---|
EN 14700: T Co1
ASME IIC SFA 5.21 / AWS A 5.21: ERCCoCr-C
| DESCRIPTION |
|---|
• Cobalt base cored wire for gas shielded metal arc hardfacing
• Co-Ci-Ni-Mo alloy deposit
• Excellent metal-to-metal wear resistance combined good corrosion resistance
| APPLICATIONS |
|---|
Stelloy 21-G is used for hardsurfacing parts subjected to a combination of impact, abrasion, compression, corrosion and high temperatures up to 900°C
The toughness of the deposit allows excellent resistance to thermal cycles and shocks
Less crack sensitive than other cobalt base alloys, Stelloy 21-G is used for building up large-scale sections
Used for integral seats and guides of large water and high-pressure valve bodies, drop forging dies, pump shafts and sleeves, hot punches etc.
| TYPICAL ALL-WELD METAL ANALYSIS |
|---|
| C | Mn | Si | Cr | Ni | Mo | Fe | Co |
|---|---|---|---|---|---|---|---|
| 0.25 | 1.00 | 1.00 | 28.5 | 3.00 | 5.50 | 4.00 | Bal. |
Structure: carbides in an austenitic matrix
| TYPICAL ALL-WELD METAL MECHANICAL PROPERTIES |
|---|
Hardness:
As welded: 33 HRC Work hardened: 47 HRC |
|---|
| CONDITIONS OF USE |
|---|
| Current type | Shielding gas | Gas flow rate | |
|---|---|---|---|
| DC+ or pulsed | EN 439 / ISO 14175: I1 (argon), M13 (Ar+1à 2 % O2) | 10 - 20 l/min | |
| OPERATING CONDITIONS |
|---|
| Diameter [mm] | Amperage [A] | Voltage [V] | Stick-out [mm] | |||
|---|---|---|---|---|---|---|
| Range | Optimum | Range | Optimum | Range | Optimum | |
| 1.2 | 100 - 250 | 200 | 16 - 29 | 28 | 15 - 30 | 10 - 25 |
| 1.6 | 140 - 350 | 250 | 16 - 30 | 28 | 15 - 30 | 10 - 25 |
Recovery: 95 %
| WELDING POSITIONS |
|---|
Flat, half up, half down
| STANDARD DIAMETERS (mm) |
|---|
1.2, 1.6, 2.0, 2.4 mm
Other diameters: please consult us
| PACKAGING |
|---|
| Diameter | ≤ 2.4 mm | ≥ 2.4 mm | |
|---|---|---|---|
| Standard packaging [EN ISO 544] | Spool : BS 300 | Coil : B 450 | Drum |
| Weight | 15 kg | 25 kg | Up to 330 kg |
Other packaging: please consult us