STELLOY Cobalt Cored Wires

welding-alloys.com 7 Typical welding procedure - Ø 1.2mm: Polarity: DC+ Welding technique: Pulsed Wire speed: 6 - 7 m/min Current: 180 - 200 A Voltage: 23 - 25 V Welding speed: 37 - 39 cm/min Stick-out: 15 mm Gas shielding: I1 (100% Ar) Gas flow: 16 - 19 l/min Typical welding procedure - Ø 1.2mm: Polarity: DC- Welding technique: CC Wire speed: 1.5 - 2.5 m/min Current: 200 - 210 A Voltage: 13 - 15 V Welding speed: 15 - 19 cm/min Gas shielding: I1 (100% Ar) TIG hot wire technology is also possible and increases the deposition rate GMAW welding process GTAW welding process Welding demo video Back to contents page